Welding Procedure Qualification

Managing the welding process

  • From choice of contractor to sign off of final documentation, we manage all your welding requirements:
  • Selection of welding contractor and welding equipment
  • Weld procedure development and optimization
  • Fabrication of girth weld qualification samples
  • Weld procedure qualification testing using both API, DNV, CSA, ISO and AS code mechanical tests, and alternative acceptance criteria testing such as CTOD and SENT, as well as sour service (SS) and SS fatigue tests
  • Tie-in and repair procedures
  • Review and approval of weld procedures and qualification records
  • Compilation of qualification records and supply of the documentation package where required